Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 223 °C | 433 °F | Injection |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |