Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 143 - 171 °C | 289 - 340 °F | |
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE) Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha.. |