Processing Properties Metric English Comments
Injection Velocity 90.0 mm/sec
3.54 in/sec
Injection molding
BASF Ultraform H 2320 006 Q600 POM
Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470.