Front Barrel Temperature 70.0 - 85.0 °C
158 - 185 °F
Barrel Inlet Temp
Perstorp Compounds 136 Urea-Formaldehyde w/ cellulose filler
A UF-based injection grade designed for hidden parts like sockets, circuit breakers, clamps, switches.Information provided by Perstorp Compounds Inc.