Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 354 - 371 °C | 670 - 700 °F | |
Oxford Polymers PEEK 450-INJ-Black PEEK Product Description: Polyetheretherketone, general purpose injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon black Special Characteristics: Precol.. |
|||
Front Barrel Temperature | 354 - 377 °C | 670 - 710 °F | |
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced Product Description: Carbon Fiber (20% Reinforced), PEEK, Polyetheretherketone, injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon fiber Special Ch.. |
|||