Processing Properties Metric English Comments
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow
Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow
Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact
Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, ..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow
Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-GP2-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Medium Flow
Polycarbonate, 5% PTFE, General Purpose, Medium Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-GP3-TFE10 Polycarbonate, 10% PTFE, High Flow, Wear Resistant
Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-GP3-TFE5 Polycarbonate, 5% PTFE, High Flow, Wear Resistant
Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
Middle Barrel Temperature 299 - 338 °C
570 - 640 °F
Polymer Resources PC-HH Polycarbonate, High Heat
Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource..
Middle Barrel Temperature 299 - 338 °C
570 - 640 °F
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized
Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow
Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow
Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
LTL Color Compounds ColorFast® PC60 Polycarbonate
6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc.
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled
High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc.
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 299 - 310 °C
570 - 590 °F
A. Schulman ComAlloy Hiloy® 714 PPS, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 299 - 310 °C
570 - 590 °F
A. Schulman ComAlloy Hiloy® 754 Glass Reinforced, Flow Enhanced, PPS Alloy, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 299 - 310 °C
570 - 590 °F
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy
Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b..
Middle Barrel Temperature 299 - 310 °C
570 - 590 °F
A. Schulman ComAlloy Hiloy® 753 Glass Reinforced, Flow Enhanced, PPS Alloy, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
LTL Color Compounds ColorFast® FRPC310 Polycarbonate, Flame-Retarded
V0-rated 10% glass-filled polycarbonate, excellent impact strengthAll information provided by LTL Color Compounders, Inc.
Middle Barrel Temperature 299 - 310 °C
570 - 590 °F
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 299 - 310 °C
570 - 590 °F
A. Schulman ComAlloy Hiloy® 756 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy
Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.