Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 246 - 279 °C | 475 - 535 °F | |
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302.. |
|||
Middle Barrel Temperature | 263 - 279 °C | 505 - 535 °F | |
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |