Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |