Processing Properties Metric English Comments
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane
Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi..
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane
Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling ..
Middle Barrel Temperature 180 - 205 °C
356 - 401 °F
Extrusion
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester
Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT..
Middle Barrel Temperature 185 - 205 °C
365 - 401 °F
Injection Molding
LG Chemical KEYFLEX BT 1030D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma..
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 85 AB Thermoplastic Polyurethane
Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma..
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling ..
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 92 AB Thermoplastic Polyurethane
Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma..
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 95 AB Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane
Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi..
Middle Barrel Temperature 195 - 205 °C
383 - 401 °F
Huntsman AVALON® 95 ABR Thermoplastic Polyurethane
Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma..