Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 182 - 200 °C | 359 - 392 °F | |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Middle Barrel Temperature | 182 - 200 °C | 359 - 392 °F | |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |