Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 121 °C | 250 °F | |
Borealis FR4847 Polyethylene Based Striping Compound FR4847 is a Polyethylene Based Striping Compound for Primary Automotive Wires. FR4847 is designed and manufactured with advanced material and processing technology to provide enhanced stabilization.. |