Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Sintering Temperature 1000 - 1300 °C
1830 - 2370 °F
Firing profile should be over 1-2 hrs with 10-20 mins at peak temperature.
Gwent Electronic Materials C2011004P5 Platinum Ink
Platinum Ink is designed for oxygen sensor applications. This is a pure platinum ink with no inorganic additions to give maximum response to oxygen. It is suitable for firing on to other high tempe..