Processing Properties | Metric | English | Comments |
---|---|---|---|
Sintering Temperature | 1900 °C | 3450 °F | or higher |
Momentive Performance Materials Titanium Diboride/Boron Nitride Composite Vacuum Metallizing Boat Intermetallic composites from Advanced Ceramics are used vacuum metallizing industry. These ceramics withstand higher operating temperatures, have lower moisture sensitivity, low thermal expansion.. |