Processing Properties | Metric | English | Comments |
---|---|---|---|
Sintering Temperature | 1250 °C @Time 10800 sec |
2280 °F @Time 3.00 hour |
|
PPT BP850 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |
|||
Sintering Temperature | 1250 °C @Time 10800 sec |
2280 °F @Time 3.00 hour |
|
PPT BP40 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |
|||
Sintering Temperature | 1250 °C @Time 10800 sec |
2280 °F @Time 3.00 hour |
|
PPT BP125HR NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |