Cure Time 70.2 min

@Temperature 25.0 °C
1.17 hour

@Temperature 77.0 °F
Tack-Free Time
3M AC-250 A-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l..