Processing Properties Metric English Comments
Cure Time 4080 min

@Thickness 5.00 mm
68.0 hour

@Thickness 0.197 in
room temp
Loctite® 5920™ RTV Silicone Sealant
LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi..