Processing Properties Metric English Comments
Cure Time 2040 min

@Temperature 16.0 °C
34.0 hour

@Temperature 60.8 °F
Full Load
Chesterton ARC 988 Composite
Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi..