Processing Properties Metric English Comments
Cure Time 720 - 1080 min

@Temperature 25.0 °C
12.0 - 18.0 hour

@Temperature 77.0 °F
Resin Technology Group KONA 871 Low Cost Epoxy Resin
Mix ratio 100 to 25 by weight.Kona 871 is a low cost epoxy resin system developed for production casting, potting, encapsulating and coating applications where easy handling, good flowability and lo..
Cure Time 720 - 1080 min

@Temperature 24.0 °C
12.0 - 18.0 hour

@Temperature 75.2 °F
BCC Products BC 7053 Epoxy Casting
BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding..