Processing Properties Metric English Comments
Cure Time 25.00 min

@Temperature 32.0 °C
0.4167 hour

@Temperature 89.6 °F
Full Load
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
Cure Time 25.00 min

@Temperature 16.0 °C
0.4167 hour

@Temperature 60.8 °F
Tack Free
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound
Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a th..
Cure Time 25.00 min

@Temperature 32.0 °C
0.4167 hour

@Temperature 89.6 °F
Full Load
Chesterton MRS 5 Metal Rebuilding System
MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we..