Processing Properties Metric English Comments
Hold Pressure 4.00 MPa
580 psi
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa..