Processing Properties | Metric | English | Comments |
---|---|---|---|
Hold Pressure | 2.76 - 5.17 MPa | 400 - 750 psi | |
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |