Processing Properties Metric English Comments
Extrusion Rate 5.50 - 7.50 g/min
5.50 - 7.50 g/min
Parker Chomerics CHO-FORM 5532 EMI Shielding Material
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 553..
Extrusion Rate 5.50 g/min
5.50 g/min
Parker Chomerics CHO-FORM 5531 EMI Shielding Material
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed..