Gel Time 8.00 min

@Temperature 120 °C
8.00 min

@Temperature 248 °F
Hot Plate
Lord Adhesives Thermosetâ„¢ MD-130 Electrically Insulating Die-Attach Adhesive
Lord MD-130 is a microelectronic grade, die-attach adhesive system for use in applications where electrical conductivity is not required. This system offers long, room temperature stability, fast cu..
Gel Time 8.00 min

@Temperature 135 °C
8.00 min

@Temperature 275 °F
50.98% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 138 °C
8.00 min

@Temperature 280 °F
64.91% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 140 °C
8.00 min

@Temperature 284 °F
75.72% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 143 °C
8.00 min

@Temperature 289 °F
82.31% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 145 °C
8.00 min

@Temperature 293 °F
85.12% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 148 °C
8.00 min

@Temperature 298 °F
87.17% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 150 °C
8.00 min

@Temperature 302 °F
89.42% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 153 °C
8.00 min

@Temperature 307 °F
88.74% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 155 °C
8.00 min

@Temperature 311 °F
89.18% Gel content
Lushan Solar EVA Film Lamination, Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 - 13.0 min

@Temperature 120 °C
8.00 - 13.0 min

@Temperature 248 °F
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix
HexPly® M47 is a toughened, self extinguishing 140ºC curing epoxy resin matrix that has been developed for the performance car market. It exhibits good strength retention at elevated temperature, ..
Gel Time 8.00 min

@Temperature 136 °C
8.00 min

@Temperature 277 °F
80.39% Gel content
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 138 °C
8.00 min

@Temperature 280 °F
83.56% Gel content
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 140 °C
8.00 min

@Temperature 284 °F
84.78% Gel content
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 143 °C
8.00 min

@Temperature 289 °F
87.59% Gel content
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..
Gel Time 8.00 min

@Temperature 145 °C
8.00 min

@Temperature 293 °F
89.23% Gel content
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure
EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu..