Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 7.00 - 9.00 min @Temperature 120 °C |
7.00 - 9.00 min @Temperature 248 °F |
|
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |