Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 4.00 min @Temperature 135 °C |
4.00 min @Temperature 275 °F |
Oven |
Lord Adhesives Thermosetâ„¢ MD-130 Electrically Insulating Die-Attach Adhesive Lord MD-130 is a microelectronic grade, die-attach adhesive system for use in applications where electrical conductivity is not required. This system offers long, room temperature stability, fast cu.. |
|||
Gel Time | 4.00 min @Temperature 136 °C |
4.00 min @Temperature 277 °F |
53.78% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 4.00 min @Temperature 138 °C |
4.00 min @Temperature 280 °F |
70..21% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 4.00 min @Temperature 140 °C |
4.00 min @Temperature 284 °F |
71.67% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 4.00 min @Temperature 143 °C |
4.00 min @Temperature 289 °F |
82.43% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 4.00 min @Temperature 145 °C |
4.00 min @Temperature 293 °F |
85.67% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |