Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 30.0 min @Temperature 180 °C |
30.0 min @Temperature 356 °F |
|
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process... |