Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | >= 240 min @Temperature 120 °C |
>= 240 min @Temperature 248 °F |
|
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process... |