Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 10.0 min @Temperature 150 °C |
10.0 min @Temperature 302 °F |
89.38% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 153 °C |
10.0 min @Temperature 307 °F |
90.26% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 155 °C |
10.0 min @Temperature 311 °F |
89.93% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 135 °C |
10.0 min @Temperature 275 °F |
66.37% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 138 °C |
10.0 min @Temperature 280 °F |
77.72% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 140 °C |
10.0 min @Temperature 284 °F |
81.8% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 143 °C |
10.0 min @Temperature 289 °F |
84.41% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 145 °C |
10.0 min @Temperature 293 °F |
87.77% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 148 °C |
10.0 min @Temperature 298 °F |
88.48% Gel content |
Lushan Solar EVA Film Lamination, Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 - 12.0 min @Temperature 110 °C |
10.0 - 12.0 min @Temperature 230 °F |
|
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |
|||
Gel Time | 10.0 min @Temperature 136 °C |
10.0 min @Temperature 277 °F |
82.79% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 138 °C |
10.0 min @Temperature 280 °F |
87.03% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 140 °C |
10.0 min @Temperature 284 °F |
86.21% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 143 °C |
10.0 min @Temperature 289 °F |
89.93% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |
|||
Gel Time | 10.0 min @Temperature 145 °C |
10.0 min @Temperature 293 °F |
90.34% Gel content |
Lushan Solar EVA Film Lamination, Low Temperature Ultra Fast Cure EVA film for encapsulating solar module Lushan series with ultra fast cure characteristic is used as encapsulate materials for photovoltaic industry. With Innovative technology, Lushan ultra fast cu.. |