Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1330 - 1430 °C | 2430 - 2610 °F | |
Wieland 1915 Wilaform Gold Yield palladium white gold alloy with beautiful grey color. Well suitable for seizing stones.Applications: chains, coin/shape, laminar decoration, tubingDental |