Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1320 - 1420 °C | 2410 - 2590 °F | |
Wieland 1751 Wilaform Palladium Approach-steady palladium alloy for nearly all purposes in decoration manufacturingApplications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Casting Temperature | 1320 °C | 2410 °F | |