Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1220 °C | 2230 °F | |
Wieland BioPortadur Casting Alloy Gold casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental |