Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1200 °C | 2190 °F | |
Wieland Porta Maximum PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |