Processing Properties | Metric | English | Comments |
---|---|---|---|
Casting Temperature | 1950 - 2150 °C | 3540 - 3900 °F | |
Wieland 1746 Wilaform Platinum Platinum alloy particularly suitable for decoration castingApplications: casting, laminar decoration, tubingDental |
|||
Casting Temperature | 1950 - 2150 °C | 3540 - 3900 °F | |
Wieland 1757 Wilaform Platinum Platinum alloy without nickel, low-priced for all kinds of decoration productionApplications: chains, laminar decoration, pipes, tubingDental |