Processing Properties Metric English Comments
Casting Temperature 1270 - 1370 °C
2320 - 2500 °F
Wieland 1916 Wilaform Gold
Hard palladium white gold alloy with beautiful grey color.Applications: casting, chains, laminar decoration, pipes, tubingDental