Polymer Property : Zone 5 = 572 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 5 250 - 300 °C
482 - 572 °F
Teknor Apex Beetle® MD21 Nylon 6, Extrusion Grade
Notes: MD21 is a medium viscosity grade of nylon 6, designed for wire coating extrusion. MD21 is heavily pigment and is designed to provide good opacity even with thin coatings. It also features a..