Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 5 | 375 - 395 °C | 707 - 743 °F | |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |