Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 410 °C | 770 °F | |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |