Processing Properties Metric English Comments
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3309HR PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass reinforced, hyd..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 4300LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300LM is a toughened 30% glass reinforced PBT that is enhanced for improved laser marking graphics.30% glass fiber, good impact strength, laser markableInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 4302LM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance, that is also enhanced for improved laser marking graphics.30% glass fiber, impact ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 5200-2 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.15% glass reinforced, high gloss, general purpose, lubricatedInfor..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Vandar® 4602Z PBT  (Unverified Data**)
4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Unreinforced, good chemical resistanceInformation provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Vandar® 4662Z PBT, 30% Glass Reinforced  (Unverified Data**)
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..
Zone 4 240 °C
464 °F
Injection Molding
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE.
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 1600A PBT, Unfilled
Celanex 1600A is a high molecular weight grade of unreinforced polybutylene terephthalate used in both extrusion and injection molding applications.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 1632Z PBT, 15% Glass Reinforced
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2000-3 PBT, Unfilled
Celanex 2000-3 is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity.. Celanex 2000-3 is a high flow material. Celanex 2000-3 contains an internal..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2000-3FC PBT, Unfilled
Celanex 2000-3FC is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity for use in food contact applications.. Celanex 2000-3FC is a high flow mater..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2008 PBT, Unfilled
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 2404 MT PBT, Medical Technology
Celanex 2404 MT Natural is an unreinforced PTFE filled PBT with improved friction, sliding, and wear properties that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administra..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX MT2008 PBT, Unfilled
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by C..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3109HR PBT, 7.5% Glass Reinforced
Celanex 3109HR is a non-lubricated, 7.5% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties, and processability.7.5% glass filledInform..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3409HR PBT, 40% Glass Reinforced
Celanex 3409HR is a non-lubricated, 40% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.To avoid hydrolytic degra..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 602AC PBT, Glass Reinforced
Celanex 602AC is a 10% fiberglass reinforced PBT that has lower warpage and improved impact over standard PBT.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a ..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese VANDAR 4602Z PBT, Unfilled
4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 6400-2 PBT, Mineral / Glass Reinforced
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2003-3 PBT, Unfilled
Celanex 2003-3 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability, and good flow characterictics. Celanex 2003-3 is a medium h..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3202-2 PBT, Glass Reinforced
Celanex 3202-2 is a 20% glass-filled Polybutylene Terephthalate that has an excellent balance of mechanical properties and processability. It contains an internal lubricant for mold release.To avoi..
Zone 4 240 - 265 °C
464 - 509 °F
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited..
Zone 4 240 °C
464 °F
Injection Molding
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube
Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE.
Zone 4 240 - 255 °C
464 - 491 °F
Celanese CELANEX 7716 PBT, 35% Mineral / Glass Reinforced
Celanex 7716 is a 35% glass/mineral reinforced, non exuding, flame retarded polybutylene terephthlate which has and excellent balance of mechanical properties and processability. Celanex 7716 is wel..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese VANDAR 2100 PBT, Unfilled
Vandar 2100 is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional stabi..
Zone 4 240 - 265 °C
464 - 509 °F
Celanese Celanex® 6407 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.30% glass/mi..
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 4302 PBT, 30% Glass Reinforced
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.Information provided by Celanese
Zone 4 240 - 260 °C
464 - 500 °F
Celanese CELANEX 4302LM PBT, 30% Glass Reinforced
Celanex 4302LM is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance, that is also enhanced for improved laser marking graphics.Information provided b..