Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 290 - 300 °C
554 - 572 °F
Celanese Celstran® PA66-GF50-0112P7,5/10 PA666, 50% Glass Reinforced  (Unverified Data**)
Material code according to ISO 1043-1: PA66PA66/6 copolymer with 50% ash content high gloss, UV stabilized, UL - listing (f1)Information provided by Celanese
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 3 290 - 305 °C
554 - 581 °F
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7177 Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7390 Polyamide 66, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7791 Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8218 Polyamide 66, with carbon fiber, toughness-modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Reduced moment of inertia compared with metal parts.Elec..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8259 Polyamide 66, with glass fiber, thermally conductive modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Emergency running property.Coil formers, duty parts in plugs and switches, ..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic st..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® NSB 90 NT Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOTECH® MR 1025 BK Polyamide 66, with mineral filler
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/15/HS Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/20/TF/5 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/30 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/CF/30/TF/15 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/GF/20/TF/10/SI/2/NC Polyamide 66, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1/XCF/40 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-0784 Polyamide 66, with glass fiber and carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-0866 Polyamide 66, with aramid reinforcement, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-0867 Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7701 Polyamide 66, with glass fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Zone 3 290 - 300 °C
554 - 572 °F
Celanese Celstran® PA66-GF40-0101P10/11 PA666, 40% Glass Reinforced
Material code according to ISO 1043-1: PA66PA66/6 Copolymer with 40% ash contentInformation provided by Celanese
Zone 3 290 - 300 °C
554 - 572 °F
Celanese Celstran® PA66-GF40-02P11 Nylon 66, 40% Glass Reinforced
Material code according to ISO 1043-1: PA66Information provided by Celanese
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7003 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Zone 3 290 - 310 °C
554 - 590 °F
Lehmann & Voss LUVOCOM® 1-8228 Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..