Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 204 - 213 °C | 400 - 415 °F | |
LyondellBasell Petrothene® LR686001 High Density Polyethylene ApplicationsPETROTHENE LR686001 is designed for use as insulation for foam/skin telephone singles, and is a natural, expandable, high density polyethylene compound containing a chemical blowing agen.. |