Polymer Property : Zone 3 = 191 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 3 179 - 191 °C
355 - 375 °F
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE..