Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 140 - 170 °C | 284 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Zone 3 | 165 - 170 °C | 329 - 338 °F | |
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane Pearlbond™ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus.. |
|||
Zone 3 | 160 - 170 °C | 320 - 338 °F | |
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane Pearlbond™ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ.. |
|||
Zone 3 | 140 - 170 °C | 284 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 3 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Polidiemme® G/220 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S.. |