Polymer Property : Zone 2 = 385 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 196 - 210 °C
385 - 410 °F
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer
PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra..
Zone 2 196 °C
385 °F
Metering Zone
Lubrizol Advanced Materials PEARLTHANE® Clear 15N80 Thermoplastic Polyurethane Elastomer
PEARLTHANE® CLEAR 15N80 is a polyether copolymer-based TPU, supplied in form of translucent, colorless, combining low hardness with excellent mechanical properties and excellent hydrolysis resist..
Zone 2 196 °C
385 °F
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas..