Polymer Property : Zone 2 = 330 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 166 °C
330 °F
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..
Zone 2 166 °C
330 °F
Axiall 3802 Vinyl Foam, Extrusion
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall..
Zone 2 166 °C
330 °F
Axiall 3801 Vinyl Foam, Extrusion
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall..
Zone 2 166 °C
330 °F
Axiall 3803 Vinyl Foam, Extrusion
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall..