Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 149 - 163 °C | 300 - 325 °F | |
LyondellBasell Petrothene® NA217080 Low Density Polyethylene ApplicationsPETROTHENE NA 217-080 is a natural low density polyethylene resin formulated for use as primary insulation for coaxial and control cable applications. NA 217-080 has also been designed .. |
|||
Zone 2 | 149 - 163 °C | 300 - 325 °F | |
LyondellBasell Petrothene® NA951080 Low Density Polyethylene ApplicationsPETROTHENE NA 951-080 is designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation. NA 951-080 is a natural, low density, medium.. |