Polymer Property : Zone 2 = 194 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 194 °C
381 °F
Extrusion
Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane
Features: High stiffness TPU alloyUses: Flat Die/Cast Sheet Extrusion, Profile Extrusion and Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided b..