Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 168 - 179 °C | 335 - 355 °F | |
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |