Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 155 - 165 °C | 311 - 329 °F | Extrusion Molding |
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon. |