Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 145 - 155 °C | 293 - 311 °F | |
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane Pearlbond™ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus.. |
|||
Zone 1 | 145 - 155 °C | 293 - 311 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten.. |