Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 138 - 177 °C | 280 - 351 °F | |
Styrolution PS-168M Polystyrene Description: Polystyrene 168M is a high heat, high molecular weight general purpose polystyrene with excellent clarity and high stiffness. Due to its high melt strength and high stiffness. PS-168M i.. |